Austenitischer rostfreier Stahl

Sandvik 253 MA

Geliefert von:

Sandvik Materials Technology

Phosphorbronze

UNS C51900 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18160 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18150 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Pure / Low Alloyed Copper

UNS C14415 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19010 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19005 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18400 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C52100 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Silver Grade

UNS C75200 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70260 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19400 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19210 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C51100 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C52400 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C51000 boway

Geliefert von:

Ningbo Boway Alloy Material

Nickel Chromium Iron Alloy

Sanicro® 28

Geliefert von:

Sandvik Materials Technology