Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 1.76 g/cm³ Show Supplier Material materials with Dichte of 1.76 g/cm³ | |
Partikelgrößenbereich | 0.76 µm Show Supplier Material materials with Partikelgrößenbereich of 0.76 µm | ||
Partikelgröße | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 20 MPa Show Supplier Material materials with Biegefestigkeit of 20 MPa |
Biegefestigkeit, transversal | 23.0 °C | 17 MPa Show Supplier Material materials with Biegefestigkeit, transversal of 17 MPa |
Druckfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Druckfestigkeit of 55 MPa |
Druckfestigkeit, transversal | 23.0 °C | 55 MPa Show Supplier Material materials with Druckfestigkeit, transversal of 55 MPa |
Elastizitätsmodul | 23.0 °C | 10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa |
Elastizitätsmodul, transversal | 23.0 °C | 8.5 GPa Show Supplier Material materials with Elastizitätsmodul, transversal of 8.5 GPa |
Hardness, Rockwell R | 23.0 °C | 93 [-] Show Supplier Material materials with Hardness, Rockwell R of 93 [-] |
Zugfestigkeit | 23.0 °C | 14 MPa Show Supplier Material materials with Zugfestigkeit of 14 MPa |
Zugfestigkeit, transversal | 23.0 °C | 12 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 12 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.15 % Show Supplier Material materials with Aschegehalt of 0.15 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.2E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 156 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 156 W/(m·K) | |
Thermal conductivity, through-plane | 23.0 °C | 140 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 140 W/(m·K) | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3.85E-6 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3.85E-6 1/K | average for 20-100°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 7.4E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 7.4E-6 Ω·m |
spezifischer Widerstand, transversal | 23.0 °C | 8.5E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand, transversal of 8.5E-6 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | CZ silicon crystal growth, Quartz, Casting molds and furnace parts for hot metal |