Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 2.83 g/cm³ Show Material materials with Dichte of 2.83 g/cm³ | AA Standards | Rod |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 70.0 - 73.0 GPa Show Material materials with Elastizitätsmodul of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium |
Schubmodule | 26.0 - 27.5 GPa Show Material materials with Schubmodule of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Schmelzpunkt | 500.0 - 650.0 °C Show Material materials with Schmelzpunkt of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 251.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 6e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Bismut | 0.4 % Show Material materials with Bismut of 0.4 % | AA Standards | Rod |
Blei | 0.2 % Show Material materials with Blei of 0.2 % | AA Standards | Rod |
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % | AA Standards | Rod |
Eisen | 0.80 % Show Material materials with Eisen of 0.80 % | AA Standards | Rod |
Kupfer | 3.9 - 5.2 % Show Material materials with Kupfer of 3.9 - 5.2 % | AA Standards | Rod |
Magnesium | 0.3 - 1.3 % Show Material materials with Magnesium of 0.3 - 1.3 % | AA Standards | Rod |
Mangan | 0.3 - 1.0 % Show Material materials with Mangan of 0.3 - 1.0 % | AA Standards | Rod |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % | AA Standards | Rod |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % | AA Standards | Rod |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | AA Standards | Rod |
Zink | 0.7 % Show Material materials with Zink of 0.7 % | AA Standards | Rod |
Zinn | 0.7 - 1.5 % Show Material materials with Zinn of 0.7 - 1.5 % | AA Standards | Rod |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |