Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.69 g/cm³ Show Material materials with Dichte of 2.69 g/cm³ | F | AA Standards |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | F | AA Standards | |
Härte, Brinell | 55.0 [-] Show Material materials with Härte, Brinell of 55.0 [-] | F | AA Standards | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||
Zugfestigkeit | 205.0 MPa Show Material materials with Zugfestigkeit of 205.0 MPa | F | AA Standards |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K | F | AA Standards | |
100 °C | 2.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K | F | AA Standards | ||
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |||
Schmelzpunkt | 630.0 - 655.0 °C Show Material materials with Schmelzpunkt of 630.0 - 655.0 °C | F | AA Standards | ||
Spezifische Wärmekapazität | 879.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | |||
Wärmeleitfähigkeit | 176 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 176 W/(m·K) | F | AA Standards |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 27000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 27000000.0 S/m | F | AA Standards |
spezifischer Widerstand | 3.7e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.7e-08 Ω·m | F | AA Standards |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Eisen | 0.10 % Show Material materials with Eisen of 0.10 % | F | AA Standards |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % | F | AA Standards |
Magnesium | 0.8 - 1.2 % Show Material materials with Magnesium of 0.8 - 1.2 % | F | AA Standards |
Mangan | 0.15 - 0.45 % Show Material materials with Mangan of 0.15 - 0.45 % | F | AA Standards |
Silizium | 0.08 % Show Material materials with Silizium of 0.08 % | F | AA Standards |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | F | AA Standards |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | F | AA Standards |
Technological properties
Property | ||
---|---|---|
Brazing | general: Lötbar mit speziellen Techniken oder bei bestimmten Anwendungen | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable | |
Workability | general (condition): good |