Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | T4 | EN 573-3, EN 755 | Rod, Tube |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3, EN 755 | Rod, Tube | A50 | |
15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3, EN 755 | Rod, Tube | A100 | ||
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3 | Profile | A50 | |
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3 | Profile | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Härte, Brinell | 20.0 °C | 50.0 [-] Show Material materials with Härte, Brinell of 50.0 [-] | T4 | EN 573-3 | Profile | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Zugfestigkeit | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | T4 | EN 573-3, EN 755 | Rod, Tube | ||
20.0 °C | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | T4 | EN 573-3 | Profile |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | T4 | EN 573-3, EN 755 | Rod, Tube | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | T4 | EN 573-3, EN 755 | Rod, Tube | ||
Schmelzpunkt | 605.0 - 655.0 °C Show Material materials with Schmelzpunkt of 605.0 - 655.0 °C | T4 | EN 573-3, EN 755 | Rod, Tube | ||
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Wärmeleitfähigkeit | 180.0 - 188.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 180.0 - 188.0 W/(m·K) | T4 | EN 573-3, EN 755 | Rod, Tube |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 27000000.0 - 28000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 27000000.0 - 28000000.0 S/m | T4 | EN 573-3, EN 755 | Rod, Tube |
spezifischer Widerstand | 3.57e-08 - 3.7e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.57e-08 - 3.7e-08 Ω·m | T4 | EN 573-3, EN 755 | Rod, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
0.3 % Show Material materials with Chrom of 0.3 % | T4 | EN 573-3 | Profile | |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | T4 | EN 573-3 | Profile |
0.35 % Show Material materials with Eisen of 0.35 % | T4 | EN 573-3, EN 755 | Rod, Tube | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
0.3 % Show Material materials with Kupfer of 0.3 % | T4 | EN 573-3 | Profile | |
Magnesium | 0.4 - 0.6 % Show Material materials with Magnesium of 0.4 - 0.6 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
0.4 - 0.7 % Show Material materials with Magnesium of 0.4 - 0.7 % | T4 | EN 573-3 | Profile | |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
0.5 % Show Material materials with Mangan of 0.5 % | T4 | EN 573-3 | Profile | |
Silizium | 0.5 - 0.9 % Show Material materials with Silizium of 0.5 - 0.9 % | T4 | EN 573-3 | Profile |
0.6 - 0.9 % Show Material materials with Silizium of 0.6 - 0.9 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube | |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
0.2 % Show Material materials with Zink of 0.2 % | T4 | EN 573-3 | Profile |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |