Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 6.0 % Show Material materials with Dehnung of 6.0 % | T66 | EN 573-3, EN 12020, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | |
8.0 % Show Material materials with Dehnung of 8.0 % | T66 | EN 573-3, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
8.0 % Show Material materials with Dehnung of 8.0 % | T66 | EN 573-3, EN 12020, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
10.0 % Show Material materials with Dehnung of 10.0 % | T66 | EN 573-3, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T66 | EN 573-3 | Profile | A50 | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T66 | EN 573-3 | Rod, Tube | A50 | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T66 | EN 573-3 | Profile | ||
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T66 | EN 573-3 | Profile | A50 | |
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T66 | EN 573-3 | Rod, Tube | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T66 | EN 573-3 | Profile | ||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
69.5 GPa Show Material materials with Elastizitätsmodul of 69.5 GPa | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
Härte, Brinell | 20.0 °C | 80.0 [-] Show Material materials with Härte, Brinell of 80.0 [-] | T66 | EN 573-3 | Profile, Rod, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.1 GPa Show Material materials with Schubmodule of 26.1 GPa | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
Zugfestigkeit | 225.0 MPa Show Material materials with Zugfestigkeit of 225.0 MPa | T66 | EN 573-3, EN 12020, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
230.0 MPa Show Material materials with Zugfestigkeit of 230.0 MPa | T66 | EN 573-3, EN 754 | Strip, Sheet, Plate, Tube, Bar | |||
245.0 MPa Show Material materials with Zugfestigkeit of 245.0 MPa | T66 | EN 573-3, EN 12020, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | T66 | EN 573-3 | Profile | ||
20.0 °C | 225.0 MPa Show Material materials with Zugfestigkeit of 225.0 MPa | T66 | EN 573-3 | Profile | ||
20.0 °C | 230.0 MPa Show Material materials with Zugfestigkeit of 230.0 MPa | T66 | EN 573-3 | Rod, Tube | ||
20.0 °C | 245.0 MPa Show Material materials with Zugfestigkeit of 245.0 MPa | T66 | EN 573-3 | Rod, Tube, Profile |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
Schmelzpunkt | 615.0 - 655.0 °C Show Material materials with Schmelzpunkt of 615.0 - 655.0 °C | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Wärmeleitfähigkeit | 193.0 - 218.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 193.0 - 218.0 W/(m·K) | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 29000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 29000000.0 - 34000000.0 S/m | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar |
spezifischer Widerstand | 2.94e-08 - 3.45e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.94e-08 - 3.45e-08 Ω·m | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | T66 | EN 573-3 | Profile, Rod, Tube |
0.35 % Show Material materials with Eisen of 0.35 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | T66 | EN 573-3, EN 12020, EN 13195, EN 754, EN 755 | Profile, Rod, Tube, Strip, Sheet, Plate, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): acceptable to poor / sufficient, friction soldering: good, soft brazing with flux: acceptable | |
Corrosion properties | Seawater: good to acceptable, weathering: good | |
Workability | Excellent workability. |