Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.69 g/cm³ Show Material materials with Dichte of 2.69 g/cm³ | T4 | EN 573-3, EN 755 | Rod, Tube |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | T4 | EN 573-3, EN 755 | Rod, Tube | A50 | |
14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3, EN 755 | Rod, Tube | A100 | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T4 | EN 573-3 | Profile, Rod | A50 | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3 | Profile, Rod | ||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | T4 | EN 573-3, EN 755 | Rod, Tube | ||
Härte, Brinell | 20.0 °C | 46.0 [-] Show Material materials with Härte, Brinell of 46.0 [-] | T4 | EN 573-3 | Profile, Rod | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Zugfestigkeit | 125.0 MPa Show Material materials with Zugfestigkeit of 125.0 MPa | T4 | EN 573-3, EN 755 | Rod, Tube | ||
20.0 °C | 125.0 MPa Show Material materials with Zugfestigkeit of 125.0 MPa | T4 | EN 573-3 | Profile, Rod |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | T4 | EN 573-3, EN 755 | Rod, Tube | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | T4 | EN 573-3, EN 755 | Rod, Tube | ||
Schmelzpunkt | 615.0 - 655.0 °C Show Material materials with Schmelzpunkt of 615.0 - 655.0 °C | T4 | EN 573-3, EN 755 | Rod, Tube | ||
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Wärmeleitfähigkeit | 193.0 - 209.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 193.0 - 209.0 W/(m·K) | T4 | EN 573-3, EN 755 | Rod, Tube |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 29000000.0 - 32000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 29000000.0 - 32000000.0 S/m | T4 | EN 573-3, EN 755 | Rod, Tube |
spezifischer Widerstand | 3.13e-08 - 3.45e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.13e-08 - 3.45e-08 Ω·m | T4 | EN 573-3, EN 755 | Rod, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T4 | EN 573-3 | Profile, Rod |
0.15 % Show Material materials with Eisen of 0.15 % | T4 | EN 573-3, EN 755 | Rod, Tube | |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Mangan | 0.05 % Show Material materials with Mangan of 0.05 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | T4 | EN 573-3, EN 755 | Profile, Rod, Tube |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |