Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | O | EN 573-3, EN 683 | Strip, Sheet |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 80.0 - 140.0 MPa Show Material materials with Zugfestigkeit of 80.0 - 140.0 MPa | O | EN 573-3, EN 683 | Strip, Sheet, Foil |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | O | EN 573-3, EN 683 | Strip, Sheet | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | O | EN 573-3, EN 683 | Strip, Sheet | ||
Schmelzpunkt | 615.0 - 655.0 °C Show Material materials with Schmelzpunkt of 615.0 - 655.0 °C | O | EN 573-3, EN 683 | Strip, Sheet | ||
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Wärmeleitfähigkeit | 197.0 - 213.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 197.0 - 213.0 W/(m·K) | O | EN 573-3, EN 683 | Strip, Sheet | ||
213.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 213.0 W/(m·K) | O | EN 573-3, EN 683 | Strip, Sheet |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 30000000.0 - 32000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 30000000.0 - 32000000.0 S/m | O | EN 573-3, EN 683 | Strip, Sheet |
32000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 32000000.0 S/m | O | EN 573-3, EN 683 | Strip, Sheet | |
spezifischer Widerstand | 3.13e-08 - 3.33e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.13e-08 - 3.33e-08 Ω·m | O | EN 573-3, EN 683 | Strip, Sheet |
3.13e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.13e-08 Ω·m | O | EN 573-3, EN 683 | Strip, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.8 % Show Material materials with Eisen of 0.8 % | O | EN 573-3 | Foil |
0.80 % Show Material materials with Eisen of 0.80 % | O | EN 573-3, EN 683 | Strip, Sheet | |
Kupfer | 0.15 - 0.4 % Show Material materials with Kupfer of 0.15 - 0.4 % | O | EN 573-3, EN 683 | Foil, Strip, Sheet |
Magnesium | 0.4 - 0.8 % Show Material materials with Magnesium of 0.4 - 0.8 % | O | EN 573-3, EN 683 | Foil, Strip, Sheet |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | O | EN 573-3, EN 683 | Foil, Strip, Sheet |
Silizium | 0.2 - 0.5 % Show Material materials with Silizium of 0.2 - 0.5 % | O | EN 573-3, EN 683 | Foil, Strip, Sheet |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | O | EN 573-3, EN 683 | Foil, Strip, Sheet |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |