Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.82 g/cm³ Show Material materials with Dichte of 2.82 g/cm³ | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 90° | 12.0 °/t Show Material materials with Biegewinkel 90° of 12.0 °/t | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Dehnung | 1.0 % Show Material materials with Dehnung of 1.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | |
2.0 % Show Material materials with Dehnung of 2.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
4.0 % Show Material materials with Dehnung of 4.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
5.0 % Show Material materials with Dehnung of 5.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
6.0 % Show Material materials with Dehnung of 6.0 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | A100 | ||
20.0 °C | 1.0 % Show Material materials with Dehnung of 1.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 1.0 % Show Material materials with Dehnung of 1.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T652 | EN 573-3 | Sheet | ||
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T652 | EN 573-3 | Flat | ||
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Härte, Brinell | 20.0 °C | 175.0 - 190.0 [-] Show Material materials with Härte, Brinell of 175.0 - 190.0 [-] | T652 | EN 573-3 | Flat | |
20.0 °C | 175.0 - 185.0 [-] Show Material materials with Härte, Brinell of 175.0 - 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 175.0 - 180.0 [-] Show Material materials with Härte, Brinell of 175.0 - 180.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 175.0 [-] Show Material materials with Härte, Brinell of 175.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 180.0 - 190.0 [-] Show Material materials with Härte, Brinell of 180.0 - 190.0 [-] | T652 | EN 573-3 | Flat | ||
20.0 °C | 180.0 - 185.0 [-] Show Material materials with Härte, Brinell of 180.0 - 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 180.0 [-] Show Material materials with Härte, Brinell of 180.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 185.0 - 190.0 [-] Show Material materials with Härte, Brinell of 185.0 - 190.0 [-] | T652 | EN 573-3 | Flat | ||
20.0 °C | 185.0 [-] Show Material materials with Härte, Brinell of 185.0 [-] | T652 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 190.0 [-] Show Material materials with Härte, Brinell of 190.0 [-] | T652 | EN 573-3 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Schubmodule | 27.1 GPa Show Material materials with Schubmodule of 27.1 GPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
Zugfestigkeit | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
505.0 MPa Show Material materials with Zugfestigkeit of 505.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
525.0 MPa Show Material materials with Zugfestigkeit of 525.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
540.0 MPa Show Material materials with Zugfestigkeit of 540.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
550.0 MPa Show Material materials with Zugfestigkeit of 550.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
560.0 MPa Show Material materials with Zugfestigkeit of 560.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
570.0 MPa Show Material materials with Zugfestigkeit of 570.0 MPa | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 505.0 MPa Show Material materials with Zugfestigkeit of 505.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 505.0 MPa Show Material materials with Zugfestigkeit of 505.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 525.0 MPa Show Material materials with Zugfestigkeit of 525.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 525.0 MPa Show Material materials with Zugfestigkeit of 525.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 540.0 MPa Show Material materials with Zugfestigkeit of 540.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 540.0 MPa Show Material materials with Zugfestigkeit of 540.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 550.0 MPa Show Material materials with Zugfestigkeit of 550.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 550.0 MPa Show Material materials with Zugfestigkeit of 550.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 560.0 MPa Show Material materials with Zugfestigkeit of 560.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 560.0 MPa Show Material materials with Zugfestigkeit of 560.0 MPa | T652 | EN 573-3 | Sheet | ||
20.0 °C | 570.0 MPa Show Material materials with Zugfestigkeit of 570.0 MPa | T652 | EN 573-3 | Flat | Transverse | |
20.0 °C | 570.0 MPa Show Material materials with Zugfestigkeit of 570.0 MPa | T652 | EN 573-3 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Schmelzpunkt | 465.0 - 655.0 °C Show Material materials with Schmelzpunkt of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Spezifische Wärmekapazität | 795.0 - 1050.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Wärmeleitfähigkeit | 121.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.05 % Show Material materials with Chrom of 0.05 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T652 | EN 573-3 | Flat, Sheet |
0.15 % Show Material materials with Eisen of 0.15 % | T652 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
Kupfer | 1.5 - 2.0 % Show Material materials with Kupfer of 1.5 - 2.0 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Magnesium | 2.1 - 2.6 % Show Material materials with Magnesium of 2.1 - 2.6 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Silizium | 0.12 % Show Material materials with Silizium of 0.12 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Titan | 0.06 % Show Material materials with Titan of 0.06 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Zink | 5.7 - 6.7 % Show Material materials with Zink of 5.7 - 6.7 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Zirkonium | 0.1 - 0.16 % Show Material materials with Zirkonium of 0.1 - 0.16 % | T652 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |