Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.69 g/cm³ Show Material materials with Dichte of 2.69 g/cm³ | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | ||
20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H111 | EN 573-3 | Rod, Flat, Tube |
Abmessung
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 0 °/t Show Material materials with Biegewinkel 180° of 0 °/t | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | according to EN 485-2 | |
0.5 °/t Show Material materials with Biegewinkel 180° of 0.5 °/t | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |||
Biegewinkel 90° | 0 °/t Show Material materials with Biegewinkel 90° of 0 °/t | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | according to EN 485-2 | |
0.5 °/t Show Material materials with Biegewinkel 90° of 0.5 °/t | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |||
Dehnung | 26 % Show Material materials with Dehnung of 26 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | according to EN 485-2, A50 | |
26.0 % Show Material materials with Dehnung of 26.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | A50 | ||
27.0 % Show Material materials with Dehnung of 27.0 % | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | |||
28.0 % Show Material materials with Dehnung of 28.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | A50 | ||
31.0 % Show Material materials with Dehnung of 31.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | A50 | ||
35.0 % Show Material materials with Dehnung of 35.0 % | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | A50 | ||
40.0 % Show Material materials with Dehnung of 40.0 % | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | |||
20.0 °C | 26.0 % Show Material materials with Dehnung of 26.0 % | H111 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 26.0 % Show Material materials with Dehnung of 26.0 % | H111 | EN 573-3 | Flat | A50 | |
20.0 °C | 27.0 % Show Material materials with Dehnung of 27.0 % | H111 | EN 573-3 | Rod, Tube | ||
20.0 °C | 28.0 % Show Material materials with Dehnung of 28.0 % | H111 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 28.0 % Show Material materials with Dehnung of 28.0 % | H111 | EN 573-3 | Flat | A50 | |
20.0 °C | 31.0 % Show Material materials with Dehnung of 31.0 % | H111 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 31.0 % Show Material materials with Dehnung of 31.0 % | H111 | EN 573-3 | Flat | A50 | |
20.0 °C | 35.0 % Show Material materials with Dehnung of 35.0 % | H111 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 35.0 % Show Material materials with Dehnung of 35.0 % | H111 | EN 573-3 | Flat | A50 | |
20.0 °C | 40.0 % Show Material materials with Dehnung of 40.0 % | H111 | EN 573-3 | Flat | ||
Elastizitätsmodul | -270.0 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube, Coil, Sheet, Strip | |
-270 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube, Coil, Sheet, Strip | ||
70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |||
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 60.0 - 70.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
20.0 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube, Coil, Sheet, Strip | ||
20 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H111 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube, Coil, Sheet, Strip | ||
50.0 °C | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
100.0 °C | 68.0 GPa Show Material materials with Elastizitätsmodul of 68.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
150.0 °C | 66.0 GPa Show Material materials with Elastizitätsmodul of 66.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
200.0 °C | 63.0 GPa Show Material materials with Elastizitätsmodul of 63.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
250.0 °C | 57.0 GPa Show Material materials with Elastizitätsmodul of 57.0 GPa | H111 | EN 573-3 | Flat, Rod, Tube | ||
300.0 °C | 50.0 GPa Show Material materials with Elastizitätsmodul of 50.0 GPa | H111 | EN 573-3 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube | ||
300 °C | 50.0 GPa Show Material materials with Elastizitätsmodul of 50.0 GPa | H111 | EN 573-3 | Flat, Strip, Sheet, Plate, Wire, Rod, Tube | ||
Härte, Brinell | 18.0 [-] Show Material materials with Härte, Brinell of 18.0 [-] | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | ||
20.0 °C | 18.0 [-] Show Material materials with Härte, Brinell of 18.0 [-] | H111 | EN 573-3 | Flat | ||
Härte, HBW | 18 [-] Show Material materials with Härte, HBW of 18 [-] | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | according to EN 485-2 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Schubmodule | 26.5 GPa Show Material materials with Schubmodule of 26.5 GPa | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
20.0 °C | 25.0 GPa Show Material materials with Schubmodule of 25.0 GPa | H111 | EN 573-3 | Rod, Flat, Tube | ||
Streckgrenze | -270 °C | 22.0 MPa Show Material materials with Streckgrenze of 22.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | RP1 |
-270.0 °C | 22.0 MPa Show Material materials with Streckgrenze of 22.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | RP1 | |
15.0 MPa Show Material materials with Streckgrenze of 15.0 MPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | RP02 | ||
15 MPa Show Material materials with Streckgrenze of 15 MPa | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | according to EN 485-2 | ||
50.0 MPa Show Material materials with Streckgrenze of 50.0 MPa | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | RP02 | ||
20.0 °C | 15.0 MPa Show Material materials with Streckgrenze of 15.0 MPa | H111 | EN 573-3 | Flat | RP02 | |
20.0 °C | 15.0 MPa Show Material materials with Streckgrenze of 15.0 MPa | H111 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 22.0 MPa Show Material materials with Streckgrenze of 22.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | RP1 | |
20 °C | 22.0 MPa Show Material materials with Streckgrenze of 22.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | RP1 | |
20.0 °C | 50.0 MPa Show Material materials with Streckgrenze of 50.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube | RP02 | |
50.0 °C | 20.0 MPa Show Material materials with Streckgrenze of 20.0 MPa | H111 | EN 573-3 | RP1 | ||
100 °C | 18.0 MPa Show Material materials with Streckgrenze of 18.0 MPa | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | RP1 | |
100.0 °C | 18.0 MPa Show Material materials with Streckgrenze of 18.0 MPa | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | RP1 | |
Zugfestigkeit | 60.0 MPa Show Material materials with Zugfestigkeit of 60.0 MPa | H111 | EN 573-3 | Strip, Sheet, Plate, Wire | ||
20.0 °C | 60.0 MPa Show Material materials with Zugfestigkeit of 60.0 MPa | H111 | EN 573-3 | Rod, Flat, Tube | ||
20.0 °C | 60.0 - 90.0 MPa Show Material materials with Zugfestigkeit of 60.0 - 90.0 MPa | H111 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Coil, Sheet, Strip | according to EN 485-2 | |
20.0 °C | 60.0 - 90.0 MPa Show Material materials with Zugfestigkeit of 60.0 - 90.0 MPa | H111 | EN 573-3 | Flat | Transverse |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |
100 °C | 0.000023 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000023 1/K | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | 20-100°C | |
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | ||
Schmelzpunkt | 659.0 °C Show Material materials with Schmelzpunkt of 659.0 °C | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | ||
Spezifische Wärmekapazität | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 921.0 J/(kg·K) | H111 | EN 573-3 | Rod, Flat, Tube | |
Wärmeleitfähigkeit | 138 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 138 W/(m·K) | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
225 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 225 W/(m·K) | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |||
20.0 °C | 215.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 215.0 W/(m·K) | H111 | EN 573-3 | Rod, Flat, Tube |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 34500000.0 - 35000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 34500000.0 - 35000000.0 S/m | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |
20.0 °C | 36400000.0 - 37000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 36400000.0 - 37000000.0 S/m | H111 | EN 573-3 | Rod, Flat, Tube | |
spezifischer Widerstand | 2.86e-08 - 2.9e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.9e-08 Ω·m | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire | |
4.9e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.9e-08 Ω·m | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Chemical properties
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Aluminium | 99.8 % Show Material materials with Aluminium of 99.8 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
Andere | 0.02 % Show Material materials with Andere of 0.02 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | Min. |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | H111 | EN 573-3 | Rod, Flat, Tube | |
0.15 % Show Material materials with Eisen of 0.15 % | H111 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Strip, Sheet, Plate, Wire, Coil, Sheet, Strip | ||
Gallium | 0.03 % Show Material materials with Gallium of 0.03 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
0.03 % Show Material materials with Kupfer of 0.03 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
0.02 % Show Material materials with Magnesium of 0.02 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Mangan | 0.02 % Show Material materials with Mangan of 0.02 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
0.02 % Show Material materials with Mangan of 0.02 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
0.15 % Show Material materials with Silizium of 0.15 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Titan | 0.02 % Show Material materials with Titan of 0.02 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
Zink | 0.06 % Show Material materials with Zink of 0.06 % | H111 | EN 573-3, EN 485 | Rod, Flat, Tube, Strip, Sheet, Plate, Wire | |
0.06 % Show Material materials with Zink of 0.06 % | H111 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges | |
Brazing | Excellent | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |