Mechanisch
Property | Temperature | Value |
---|---|---|
Zugfestigkeit | 20.0 °C | 160 - 200 MPa Show Material materials with Zugfestigkeit of 160 - 200 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 99.5 % Show Material materials with Aluminium of 99.5 % |
Bor | 0.05 % Show Material materials with Bor of 0.05 % |
Chrom | 0.01 % Show Material materials with Chrom of 0.01 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Gallium | 0.03 % Show Material materials with Gallium of 0.03 % |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % |
Mangan | 0.01 % Show Material materials with Mangan of 0.01 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.05 % Show Material materials with Zink of 0.05 % |