Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 72.5 GPa Show Material materials with Elastizitätsmodul of 72.5 GPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Schubmodule | 27.2 GPa Show Material materials with Schubmodule of 27.2 GPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Zugfestigkeit | 200.0 - 260.0 MPa Show Material materials with Zugfestigkeit of 200.0 - 260.0 MPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
200.0 - 400.0 MPa Show Material materials with Zugfestigkeit of 200.0 - 400.0 MPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | ||
Schmelzpunkt | 512.0 - 650.0 °C Show Material materials with Schmelzpunkt of 512.0 - 650.0 °C | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | ||
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium | ||||
Wärmeleitfähigkeit | 130.0 - 200.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 200.0 W/(m·K) | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 28000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 28000000.0 S/m | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
spezifischer Widerstand | 3.57e-08 - 5.56e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.57e-08 - 5.56e-08 Ω·m | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Eisen | 0.70 % Show Material materials with Eisen of 0.70 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Kupfer | 3.5 - 4.5 % Show Material materials with Kupfer of 3.5 - 4.5 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Magnesium | 0.4 - 1.0 % Show Material materials with Magnesium of 0.4 - 1.0 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Mangan | 0.4 - 1.0 % Show Material materials with Mangan of 0.4 - 1.0 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: acceptable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) acceptable (O) / acceptable (O) |