Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.77 g/cm³ Show Material materials with Dichte of 2.77 g/cm³ | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20.0 °C | 2.77 g/cm³ Show Material materials with Dichte of 2.77 g/cm³ | T851 | EN 573-3 | Rod, Sheet, Flat |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 90° | 5.0 °/t Show Material materials with Biegewinkel 90° of 5.0 °/t | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
7.0 °/t Show Material materials with Biegewinkel 90° of 7.0 °/t | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |||
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | T851 | EN 573-3, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | A50 | |
3.0 % Show Material materials with Dehnung of 3.0 % | T851 | EN 573-3, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | A100 | ||
4.0 % Show Material materials with Dehnung of 4.0 % | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | A50 | ||
5.0 % Show Material materials with Dehnung of 5.0 % | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | A50 | ||
6.0 % Show Material materials with Dehnung of 6.0 % | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | A50 | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T851 | EN 573-3 | Rod | A50 | |
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | T851 | EN 573-3 | Rod | ||
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | T851 | EN 573-3 | Rod | A50 | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T851 | EN 573-3 | Sheet, Flat, Rod | ||
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T851 | EN 573-3 | Flat | Transverse | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T851 | EN 573-3 | Flat | A50 | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T851 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T851 | EN 573-3 | Flat | A50 | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T851 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T851 | EN 573-3 | Transverse | ||
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T851 | EN 573-3 | Transverse | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T851 | EN 573-3 | Sheet | A50 Transverse | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T851 | EN 573-3 | Sheet | A50 Transverse | |
Elastizitätsmodul | 73.0 GPa Show Material materials with Elastizitätsmodul of 73.0 GPa | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
20.0 °C | 70.0 - 74.5 GPa Show Material materials with Elastizitätsmodul of 70.0 - 74.5 GPa | T851 | EN 573-3 | Rod, Sheet, Flat | ||
Härte, Brinell | 136.0 [-] Show Material materials with Härte, Brinell of 136.0 [-] | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
137.0 [-] Show Material materials with Härte, Brinell of 137.0 [-] | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |||
138.0 [-] Show Material materials with Härte, Brinell of 138.0 [-] | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |||
20.0 °C | 130.0 [-] Show Material materials with Härte, Brinell of 130.0 [-] | T851 | EN 573-3 | Rod | ||
20.0 °C | 136.0 [-] Show Material materials with Härte, Brinell of 136.0 [-] | T851 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 136.0 - 138.0 [-] Show Material materials with Härte, Brinell of 136.0 - 138.0 [-] | T851 | EN 573-3 | Flat | ||
20.0 °C | 136.0 - 137.0 [-] Show Material materials with Härte, Brinell of 136.0 - 137.0 [-] | T851 | EN 573-3 | Flat | ||
20.0 °C | 137.0 - 138.0 [-] Show Material materials with Härte, Brinell of 137.0 - 138.0 [-] | T851 | EN 573-3 | Flat | ||
20.0 °C | 137.0 [-] Show Material materials with Härte, Brinell of 137.0 [-] | T851 | EN 573-3 | Flat | ||
20.0 °C | 138.0 [-] Show Material materials with Härte, Brinell of 138.0 [-] | T851 | EN 573-3 | Flat | ||
Plane-Strain Fracture Toughnes | -196.0 °C | 24.4 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 24.4 MPa·√m | T851 | EN 573-3 | ||
20.0 °C | 18.0 - 24.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 18.0 - 24.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
20.0 °C | 18.0 - 23.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 18.0 - 23.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
20.0 °C | 18.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 18.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
20.0 °C | 22.3 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.3 MPa·√m | T851 | EN 573-3 | |||
20.0 °C | 23.0 - 24.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 23.0 - 24.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
20.0 °C | 23.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 23.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
20.0 °C | 24.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 24.0 MPa·√m | T851 | EN 573-3 | Sheet | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Schubmodule | 27.4 GPa Show Material materials with Schubmodule of 27.4 GPa | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
20.0 °C | 27.0 - 28.0 GPa Show Material materials with Schubmodule of 27.0 - 28.0 GPa | T851 | EN 573-3 | Rod, Sheet, Flat | ||
Streckgrenze | -196.0 °C | 444.0 MPa Show Material materials with Streckgrenze of 444.0 MPa | T851 | EN 573-3 | ||
395.0 MPa Show Material materials with Streckgrenze of 395.0 MPa | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | RP02 | ||
400.0 MPa Show Material materials with Streckgrenze of 400.0 MPa | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | RP02 | ||
20.0 °C | 275.0 MPa Show Material materials with Streckgrenze of 275.0 MPa | T851 | EN 573-3 | Sheet | RP02 Transverse | |
20.0 °C | 285.0 MPa Show Material materials with Streckgrenze of 285.0 MPa | T851 | EN 573-3 | RP02 Transverse | ||
20.0 °C | 290.0 MPa Show Material materials with Streckgrenze of 290.0 MPa | T851 | EN 573-3 | RP02 Transverse | ||
20.0 °C | 395.0 MPa Show Material materials with Streckgrenze of 395.0 MPa | T851 | EN 573-3 | Sheet | RP02 | |
20.0 °C | 395.0 MPa Show Material materials with Streckgrenze of 395.0 MPa | T851 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 400.0 MPa Show Material materials with Streckgrenze of 400.0 MPa | T851 | EN 573-3 | Rod, Flat | RP02 | |
20.0 °C | 400.0 MPa Show Material materials with Streckgrenze of 400.0 MPa | T851 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 444.0 MPa Show Material materials with Streckgrenze of 444.0 MPa | T851 | EN 573-3 | |||
20.0 °C | 455.0 MPa Show Material materials with Streckgrenze of 455.0 MPa | T851 | EN 573-3 | Sheet | ||
Zugfestigkeit | 455.0 MPa Show Material materials with Zugfestigkeit of 455.0 MPa | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T851 | EN 573-3, EN 485 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |||
20.0 °C | 400.0 MPa Show Material materials with Zugfestigkeit of 400.0 MPa | T851 | EN 573-3 | Transverse | ||
20.0 °C | 420.0 MPa Show Material materials with Zugfestigkeit of 420.0 MPa | T851 | EN 573-3 | Transverse | ||
20.0 °C | 425.0 MPa Show Material materials with Zugfestigkeit of 425.0 MPa | T851 | EN 573-3 | Sheet | Transverse | |
20.0 °C | 455.0 MPa Show Material materials with Zugfestigkeit of 455.0 MPa | T851 | EN 573-3 | Sheet, Rod, Flat | ||
20.0 °C | 455.0 MPa Show Material materials with Zugfestigkeit of 455.0 MPa | T851 | EN 573-3 | Flat | Transverse | |
20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T851 | EN 573-3 | Flat | ||
20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T851 | EN 573-3 | Flat | Transverse |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | -50 °C | 2.11e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar |
20 °C | 2.11e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20 °C | 2.2899999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2899999999999998e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20 °C | 2.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20 °C | 2.4699999999999997e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4699999999999997e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
100 °C | 2.2899999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2899999999999998e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
200 °C | 2.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.38e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
300 °C | 2.4699999999999997e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4699999999999997e-05 1/K | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
Schmelzpunkt | 505.0 - 640.0 °C Show Material materials with Schmelzpunkt of 505.0 - 640.0 °C | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
505.0 - 635.0 °C Show Material materials with Schmelzpunkt of 505.0 - 635.0 °C | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | ||
Spezifische Wärmekapazität | 875.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 875.0 J/(kg·K) | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20.0 °C | 875.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 875.0 J/(kg·K) | T851 | EN 573-3 | Rod, Sheet, Flat | |
Wärmeleitfähigkeit | 121.0 - 193.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 121.0 - 193.0 W/(m·K) | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20.0 °C | 130.0 - 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 150.0 W/(m·K) | T851 | EN 573-3, EN 485, EN 754 | Rod, Sheet, Flat, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 17000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 17000000.0 - 29000000.0 S/m | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
20.0 °C | 18000000.0 - 21000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 21000000.0 S/m | T851 | EN 573-3, EN 485, EN 754 | Rod, Sheet, Flat, Strip, Plate, Forging, Tube, Welded Tube, Bar | |
spezifischer Widerstand | 3.45e-08 - 5.88e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.45e-08 - 5.88e-08 Ω·m | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
4.76e-08 - 5.56e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.76e-08 - 5.56e-08 Ω·m | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | T851 | EN 573-3 | Sheet, Flat, Rod |
0.50 % Show Material materials with Eisen of 0.50 % | T851 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Forging, Tube, Welded Tube, Bar | |
Kupfer | 3.8 - 4.9 % Show Material materials with Kupfer of 3.8 - 4.9 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Mangan | 0.3 - 0.9 % Show Material materials with Mangan of 0.3 - 0.9 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | T851 | EN 573-3, EN 485, EN 754 | Sheet, Flat, Rod, Strip, Plate, Forging, Tube, Welded Tube, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: acceptable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: poor | |
Workability | Bending / Spinning (cold): sufficient (O) / acceptable (O), Impact extrusion (cold): acceptable (O), Deep drawing / upsetting (Condition) acceptable (O) / sufficient (O) |