Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | ||
Härte, Brinell | 150.0 [-] Show Material materials with Härte, Brinell of 150.0 [-] | T61 | Pink Sheets, ASTM B955 | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | ||
Zugfestigkeit | 510.0 MPa Show Material materials with Zugfestigkeit of 510.0 MPa | T61 | Pink Sheets, ASTM B955 |
Thermisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium | ||
Schmelzpunkt | 477.0 - 635.0 °C Show Material materials with Schmelzpunkt of 477.0 - 635.0 °C | T61 | Pink Sheets, ASTM B955 | |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | ||
Wärmeleitfähigkeit | 100.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chrom | 0.18 - 0.28 % Show Material materials with Chrom of 0.18 - 0.28 % | T61 | Pink Sheets, ASTM B955 |
Eisen | 0.50 % Show Material materials with Eisen of 0.50 % | T61 | Pink Sheets, ASTM B955 |
Kupfer | 1.2 - 2.0 % Show Material materials with Kupfer of 1.2 - 2.0 % | T61 | Pink Sheets, ASTM B955 |
Magnesium | 2.1 - 2.9 % Show Material materials with Magnesium of 2.1 - 2.9 % | T61 | Pink Sheets, ASTM B955 |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % | T61 | Pink Sheets, ASTM B955 |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | T61 | Pink Sheets, ASTM B955 |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | T61 | Pink Sheets, ASTM B955 |
Zink | 5.1 - 6.1 % Show Material materials with Zink of 5.1 - 6.1 % | T61 | Pink Sheets, ASTM B955 |