Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T1 | EN 1706 | Casting | |
Elastizitätsmodul | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Härte, Brinell | 90.0 [-] Show Material materials with Härte, Brinell of 90.0 [-] | T1 | EN 1706 | Casting | |
100.0 [-] Show Material materials with Härte, Brinell of 100.0 [-] | T1 | EN 1706 | Casting | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Zugfestigkeit | 210.0 MPa Show Material materials with Zugfestigkeit of 210.0 MPa | T1 | EN 1706 | Casting | |
260.0 MPa Show Material materials with Zugfestigkeit of 260.0 MPa | T1 | EN 1706 | Casting |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | T1 | EN 1706 | Casting | |
100 °C | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | T1 | EN 1706 | Casting | ||
Schmelzpunkt | 550.0 - 645.0 °C Show Material materials with Schmelzpunkt of 550.0 - 645.0 °C | Typical for Cast 7xx.x Series Aluminium | ||||
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | ||||
Wärmeleitfähigkeit | 120.0 - 130.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 - 130.0 W/(m·K) | T1 | EN 1706 | Casting |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 17000000.0 - 20000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 17000000.0 - 20000000.0 S/m | T1 | EN 1706 | Casting |
spezifischer Widerstand | 5e-08 - 5.88e-08 Ω·m Show Material materials with spezifischer Widerstand of 5e-08 - 5.88e-08 Ω·m | T1 | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 78.8 % Show Material materials with Aluminium of 78.8 % | T1 | EN 1706 | |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % | T1 | EN 1706 | |
0.30 % Show Material materials with Eisen of 0.30 % | T1 | EN 1706 | Casting | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T1 | EN 1706 | Casting |
Magnesium | 0.2 - 0.5 % Show Material materials with Magnesium of 0.2 - 0.5 % | T1 | EN 1706 | Casting |
Mangan | 0.15 % Show Material materials with Mangan of 0.15 % | T1 | EN 1706 | Casting |
Silizium | 7.5 - 9.5 % Show Material materials with Silizium of 7.5 - 9.5 % | T1 | EN 1706 | Casting |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | T1 | EN 1706 | Casting |
Zink | 9.0 - 10.5 % Show Material materials with Zink of 9.0 - 10.5 % | T1 | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: acceptable | |
General machinability | as cast: excellent | |
Processing methods | permanent mould casting, separately cast test sample |