Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Härte, Brinell | 85.0 [-] Show Material materials with Härte, Brinell of 85.0 [-] | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Zugfestigkeit | 220.0 MPa Show Material materials with Zugfestigkeit of 220.0 MPa | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium | |||
Schmelzpunkt | 604.0 - 643.0 °C Show Material materials with Schmelzpunkt of 604.0 - 643.0 °C | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | |||
Wärmeleitfähigkeit | 100.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.06 - 0.2 % Show Material materials with Chrom of 0.06 - 0.2 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Magnesium | 0.8 - 1.0 % Show Material materials with Magnesium of 0.8 - 1.0 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Titan | 0.1 - 0.2 % Show Material materials with Titan of 0.1 - 0.2 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Zink | 6.5 - 7.5 % Show Material materials with Zink of 6.5 - 7.5 % | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting |