Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil |
2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | O | EN 573-3, EN 546 | Foil |
Abmessung
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 69.0 - 72.0 GPa Show Material materials with Elastizitätsmodul of 69.0 - 72.0 GPa | Typical for Wrought 8000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 60.0 - 100.0 MPa Show Material materials with Zugfestigkeit of 60.0 - 100.0 MPa | O | EN 573-3, EN 546 | Foil | |
20.0 °C | 60.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 60.0 - 105.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 60.0 - 110.0 MPa Show Material materials with Zugfestigkeit of 60.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 65.0 - 105.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 65.0 - 100.0 MPa Show Material materials with Zugfestigkeit of 65.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 110.0 MPa Show Material materials with Zugfestigkeit of 65.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 110.0 MPa Show Material materials with Zugfestigkeit of 70.0 - 110.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 70.0 - 100.0 MPa Show Material materials with Zugfestigkeit of 70.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 70.0 - 105.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 110.0 MPa Show Material materials with Zugfestigkeit of 75.0 - 110.0 MPa | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 573-3, EN 546 | Coil, Foil, Foil | ||
20.0 °C | 75.0 - 100.0 MPa Show Material materials with Zugfestigkeit of 75.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 75.0 - 105.0 MPa | O | EN 573-3 | Foil |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 0.000024 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000024 1/K | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Schmelzpunkt | 645.0 - 655.0 °C Show Material materials with Schmelzpunkt of 645.0 - 655.0 °C | Typical for Wrought 8000 Series Aluminium | ||||
Spezifische Wärmekapazität | 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Wärmeleitfähigkeit | 167.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 167.0 - 220.0 W/(m·K) | Typical for Wrought 8000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 28000000.0 - 35000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 28000000.0 - 35000000.0 S/m | Typical for Wrought 8000 Series Aluminium |
spezifischer Widerstand | 2.8e-08 - 3.5e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.8e-08 - 3.5e-08 Ω·m | Typical for Wrought 8000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.03 % Show Material materials with Chrom of 0.03 % | O | EN 573-3, EN 546 | Foil |
0.03 % Show Material materials with Chrom of 0.03 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Eisen | 1.1 - 1.7 % Show Material materials with Eisen of 1.1 - 1.7 % | O | EN 573-3, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Foil, Coil, Foil |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Kupfer of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Magnesium | 0.01 % Show Material materials with Magnesium of 0.01 % | O | EN 573-3, EN 546 | Foil |
0.01 % Show Material materials with Magnesium of 0.01 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Mangan | 0.03 % Show Material materials with Mangan of 0.03 % | O | EN 573-3, EN 546 | Foil |
0.03 % Show Material materials with Mangan of 0.03 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | O | EN 573-3, EN 546 | Foil |
0.4 % Show Material materials with Silizium of 0.4 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Titan of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Zink of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil |
Technological properties
Property | ||
---|---|---|
Application areas | Foil stock: Foil app | |
Workability | Excellent |