Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
20.0 °C | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | H24 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Coil, Sheet |
Abmessung
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Dicke | 0.04 mm Show Material materials with Dicke of 0.04 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | 0.04 mm | Coil, Sheet |
1.5 mm Show Material materials with Dicke of 1.5 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | 1.5 mm | Coil, Sheet |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 1.5 °/t Show Material materials with Biegewinkel 180° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
1.5 °/t Show Material materials with Biegewinkel 180° of 1.5 °/t | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
Biegewinkel 90° | 0.5 °/t Show Material materials with Biegewinkel 90° of 0.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
0.5 °/t Show Material materials with Biegewinkel 90° of 0.5 °/t | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
1.0 °/t Show Material materials with Biegewinkel 90° of 1.0 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | |||
1.5 °/t Show Material materials with Biegewinkel 90° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | |||
Dehnung | 1.0 - 3.0 % Show Material materials with Dehnung of 1.0 - 3.0 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | A50 | |
3.0 % Show Material materials with Dehnung of 3.0 % | H24 | EN 573-3, EN 546 | Strip, Sheet, Plate, Welded Tube | A50 | ||
4.0 % Show Material materials with Dehnung of 4.0 % | H24 | EN 573-3, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | A50 | ||
7.0 % Show Material materials with Dehnung of 7.0 % | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | A100 | ||
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | H24 | EN 573-3 | Foil | A100 | |
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | H24 | EN 573-3 | Foil | A50 | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | H24 | EN 573-3 | Foil | A100 | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | H24 | EN 573-3 | Flat, Foil | A50 | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | H24 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | H24 | EN 573-3 | Seamless Tube | ||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |||
Härte, Brinell | 52.0 [-] Show Material materials with Härte, Brinell of 52.0 [-] | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 52.0 [-] Show Material materials with Härte, Brinell of 52.0 [-] | H24 | EN 573-3 | Flat | ||
Härte, HBW | 53 [-] Show Material materials with Härte, HBW of 53 [-] | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
20.0 °C | 26.5 GPa Show Material materials with Schubmodule of 26.5 GPa | H24 | EN 573-3 | Foil, Flat, Seamless Tube | ||
Streckgrenze | 45 MPa Show Material materials with Streckgrenze of 45 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | RP02 | ||
175.0 MPa Show Material materials with Streckgrenze of 175.0 MPa | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | RP02 | ||
20.0 °C | 130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H24 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H24 | EN 573-3 | Flat | RP02 | |
20.0 °C | 175.0 MPa Show Material materials with Streckgrenze of 175.0 MPa | H24 | EN 573-3 | Seamless Tube | RP02 | |
Zugfestigkeit | 125.0 - 225.0 MPa Show Material materials with Zugfestigkeit of 125.0 - 225.0 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
200.0 MPa Show Material materials with Zugfestigkeit of 200.0 MPa | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | |||
20.0 °C | 170.0 - 215.0 MPa Show Material materials with Zugfestigkeit of 170.0 - 215.0 MPa | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 170.0 - 215.0 MPa Show Material materials with Zugfestigkeit of 170.0 - 215.0 MPa | H24 | EN 573-3 | Flat | Transverse | |
20.0 °C | 180.0 - 225.0 MPa Show Material materials with Zugfestigkeit of 180.0 - 225.0 MPa | H24 | EN 573-3, EN 546 | Foil, Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 200.0 MPa Show Material materials with Zugfestigkeit of 200.0 MPa | H24 | EN 573-3 | Seamless Tube |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | ||
100 °C | 0.000024 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000024 1/K | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | 20-100°C | |
Schmelzpunkt | 630.0 - 654.0 °C Show Material materials with Schmelzpunkt of 630.0 - 654.0 °C | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | ||
Spezifische Wärmekapazität | 20.0 °C | 893.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 J/(kg·K) | H24 | EN 573-3 | Foil, Flat, Seamless Tube | |
Wärmeleitfähigkeit | 160.0 - 190.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160.0 - 190.0 W/(m·K) | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | ||
172 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 172 W/(m·K) | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
20.0 °C | 200.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 200.0 W/(m·K) | H24 | EN 573-3 | Foil, Flat, Seamless Tube |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 25000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 25000000.0 S/m | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
20.0 °C | 28000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 28000000.0 S/m | H24 | EN 573-3 | Foil, Flat, Seamless Tube | |
spezifischer Widerstand | 3.7999999999999996e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.7999999999999996e-08 Ω·m | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
4e-08 - 4.35e-08 Ω·m Show Material materials with spezifischer Widerstand of 4e-08 - 4.35e-08 Ω·m | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.1 % Show Material materials with Chrom of 0.1 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H24 | EN 573-3 | Foil, Flat, Seamless Tube |
0.70 % Show Material materials with Eisen of 0.70 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
0.7 % Show Material materials with Eisen of 0.7 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.3 % Show Material materials with Kupfer of 0.3 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Magnesium | 0.2 - 0.6 % Show Material materials with Magnesium of 0.2 - 0.6 % | H24 | EN 573-3, EN 1592, EN 485, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube, Coil, Sheet |
Mangan | 1.0 - 1.5 % Show Material materials with Mangan of 1.0 - 1.5 % | H24 | EN 573-3, EN 1592, EN 485, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube, Coil, Sheet |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.6 % Show Material materials with Silizium of 0.6 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.25 % Show Material materials with Zink of 0.25 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Electronic devices: Housing of devices; Insulation; Cosmetics: Cosmetics pieces | |
Brazing | Good | |
Corrosion properties | Seawater: very good, weathering: very good | |
Welding | Good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) very good (O) / acceptable (H12) |