Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.73 g/cm³ Show Material materials with Dichte of 2.73 g/cm³ | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet |
Abmessung
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 0 °/t Show Material materials with Biegewinkel 180° of 0 °/t | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
Biegewinkel 90° | 0 °/t Show Material materials with Biegewinkel 90° of 0 °/t | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
Dehnung | 1 % Show Material materials with Dehnung of 1 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | A50 | |
20.0 °C | 18.0 % Show Material materials with Dehnung of 18.0 % | O | EN 573-3 | Sheet | A50 | |
20.0 °C | 22.0 % Show Material materials with Dehnung of 22.0 % | O | EN 573-3 | Tube | ||
20.0 °C | 23.0 % Show Material materials with Dehnung of 23.0 % | O | EN 573-3 | Sheet | A50 | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
Härte, HBW | 27 [-] Show Material materials with Härte, HBW of 27 [-] | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Schubmodule | 26.5 GPa Show Material materials with Schubmodule of 26.5 GPa | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
Streckgrenze | 35 MPa Show Material materials with Streckgrenze of 35 MPa | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
20.0 °C | 35.0 MPa Show Material materials with Streckgrenze of 35.0 MPa | O | EN 573-3 | Tube, Sheet | RP02 | |
Zugfestigkeit | 90 MPa Show Material materials with Zugfestigkeit of 90 MPa | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | ||
20.0 °C | 90.0 MPa Show Material materials with Zugfestigkeit of 90.0 MPa | O | EN 573-3 | Sheet | ||
20.0 °C | 95.0 MPa Show Material materials with Zugfestigkeit of 95.0 MPa | O | EN 573-3 | Tube | ||
20.0 °C | 100.0 MPa Show Material materials with Zugfestigkeit of 100.0 MPa | O | EN 573-3 | Sheet |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 0.000023 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000023 1/K | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | 20-100°C |
Schmelzpunkt | 629.0 - 654.0 °C Show Material materials with Schmelzpunkt of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium | ||||
Spezifische Wärmekapazität | 893.0 - 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium | ||||
Wärmeleitfähigkeit | 176 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 176 W/(m·K) | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet |
Elektrisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium | |||
spezifischer Widerstand | 4.3e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.3e-08 Ω·m | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | O | EN 573-3 | Sheet, Tube |
0.1 % Show Material materials with Chrom of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | O | EN 573-3 | Sheet, Tube |
0.7 % Show Material materials with Eisen of 0.7 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | O | EN 573-3 | Sheet, Tube |
0.1 % Show Material materials with Kupfer of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | |
Magnesium | 0.3 % Show Material materials with Magnesium of 0.3 % | O | EN 573-3 | Sheet, Tube |
0.3 % Show Material materials with Magnesium of 0.3 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | |
Mangan | 0.7 - 1.4 % Show Material materials with Mangan of 0.7 - 1.4 % | O | EN 573-3, EN 573-1, EN 573-2, EN 573-3 | Sheet, Tube, Coil, Sheet |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | O | EN 573-3 | Sheet, Tube |
0.5 % Show Material materials with Silizium of 0.5 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet | |
Titan | 0.1 Show Material materials with Titan of 0.1 | O | EN 573-3 | Sheet, Tube |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | O | EN 573-3 | Sheet, Tube |
0.2 % Show Material materials with Zink of 0.2 % | O | EN 573-1, EN 573-2, EN 573-3 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | Very Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing Quality; Heat exchangers: Fins, Heat exchangers; Tubes: Flexible tube, Pipes; Cosmetics: Cosmetics pieces; Semi-rigid and corrugated: Smooth wall; Components: Automotive fins, Heat exchangers | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |