Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H28 | EN 573-3, EN 541 | Strip, Sheet, Plate |
Abmessung
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Streckgrenze | 120.0 - 220.0 MPa Show Material materials with Streckgrenze of 120.0 - 220.0 MPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 170.0 - 220.0 MPa Show Material materials with Streckgrenze of 170.0 - 220.0 MPa | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate | RP02 | |
Zugfestigkeit | 150.0 - 240.0 MPa Show Material materials with Zugfestigkeit of 150.0 - 240.0 MPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 190.0 - 240.0 MPa Show Material materials with Zugfestigkeit of 190.0 - 240.0 MPa | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 0.000024 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000024 1/K | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | 20-100°C |
Schmelzpunkt | 629.0 - 654.0 °C Show Material materials with Schmelzpunkt of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium | ||||
Spezifische Wärmekapazität | 893.0 - 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium | ||||
Wärmeleitfähigkeit | 172 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 172 W/(m·K) | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Elektrisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium | |||
spezifischer Widerstand | 3.7999999999999996e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.7999999999999996e-08 Ω·m | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.2 % Show Material materials with Chrom of 0.2 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H28 | EN 573-3 | Sheet |
0.7 % Show Material materials with Eisen of 0.7 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
0.70 % Show Material materials with Eisen of 0.70 % | H28 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.3 % Show Material materials with Kupfer of 0.3 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | H28 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Mangan | 0.3 - 0.8 % Show Material materials with Mangan of 0.3 - 0.8 % | H28 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.6 % Show Material materials with Silizium of 0.6 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.25 % Show Material materials with Zink of 0.25 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Closures: Short cups; Food can: Body, Lids; Semi-rigid and corrugated: Pet food | |
Brazing | Good | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |