Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.73 g/cm³ Show Material materials with Dichte of 2.73 g/cm³ | H48 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
20.0 °C | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H48 | EN 573-3 | Sheet |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H48 | EN 573-3, EN 541 | Strip, Sheet, Plate | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 26.5 Show Material materials with Schubmodule of 26.5 | H48 | EN 573-3 | Sheet | |
Zugfestigkeit | 20.0 °C | 180.0 - 230.0 MPa Show Material materials with Zugfestigkeit of 180.0 - 230.0 MPa | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium | ||||
Schmelzpunkt | 629.0 - 654.0 °C Show Material materials with Schmelzpunkt of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium | ||||
Spezifische Wärmekapazität | 20.0 °C | 893.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 J/(kg·K) | H48 | EN 573-3 | Sheet | |
Wärmeleitfähigkeit | 20.0 °C | 200.0 Show Material materials with Wärmeleitfähigkeit of 200.0 | H48 | EN 573-3 | Sheet |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 28000000.0 Show Material materials with Elektrische Leitfähigkeit of 28000000.0 | H48 | EN 573-3 | Sheet | |
spezifischer Widerstand | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.45 % Show Material materials with Eisen of 0.45 % | H48 | EN 573-3 | Sheet |
0.45 % Show Material materials with Eisen of 0.45 % | H48 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Mangan | 0.4 - 0.8 % Show Material materials with Mangan of 0.4 - 0.8 % | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | H48 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): very good / very good, Impact extrusion (cold): good, Deep drawing / upsetting (Condition) very good (O) / very good (H12) |