Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.71 g/cm³ Show Material materials with Dichte of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 71.0 - 75.0 GPa Show Material materials with Elastizitätsmodul of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Zugfestigkeit | 140.0 MPa Show Material materials with Zugfestigkeit of 140.0 MPa | T4 | Pink Sheets, ASTM B108 | Casting |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-05 - 2.2e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium | |||
Schmelzpunkt | 574.0 - 618.0 °C Show Material materials with Schmelzpunkt of 574.0 - 618.0 °C | T4 | Pink Sheets, ASTM B108 | Casting | |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium | |||
Wärmeleitfähigkeit | 130.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.20 % Show Material materials with Eisen of 0.20 % | T4 | Pink Sheets, ASTM B108 | Casting |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T4 | Pink Sheets, ASTM B108 | Casting |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % | T4 | Pink Sheets, ASTM B108 | Casting |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T4 | Pink Sheets, ASTM B108 | Casting |
Silizium | 6.5 - 7.5 % Show Material materials with Silizium of 6.5 - 7.5 % | T4 | Pink Sheets, ASTM B108 | Casting |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | T4 | Pink Sheets, ASTM B108 | Casting |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | T4 | Pink Sheets, ASTM B108 | Casting |