Chemical properties
Property | Value |
---|---|
Bismut | 0.4 % Show Material materials with Bismut of 0.4 % |
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Kupfer | 4.5 % Show Material materials with Kupfer of 4.5 % |
Magnesium | 1.1 % Show Material materials with Magnesium of 1.1 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Titan | 0.2 % Show Material materials with Titan of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 1.3 % Show Material materials with Zinn of 1.3 % |