Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 2.65 g/cm³ Show Material materials with Dichte of 2.65 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 65 - 75 GPa Show Material materials with Elastizitätsmodul of 65 - 75 GPa |
Chemical properties
Property | Value |
---|---|
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Magnesium | 0.08 % Show Material materials with Magnesium of 0.08 % |
Mangan | 0.6 % Show Material materials with Mangan of 0.6 % |
Silizium | 10.5 % Show Material materials with Silizium of 10.5 % |
Titan | 0.06 % Show Material materials with Titan of 0.06 % |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % |
Zink | 0.07 % Show Material materials with Zink of 0.07 % |
Zirkonium | 0.3 % Show Material materials with Zirkonium of 0.3 % |