Thermisch
Property | Value |
---|---|
Schmelzpunkt | 557 - 613 °C Show Material materials with Schmelzpunkt of 557 - 613 °C |
Chemical properties
Property | Value |
---|---|
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % |
Magnesium | 0.45 % Show Material materials with Magnesium of 0.45 % |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % |
Silizium | 7.5 % Show Material materials with Silizium of 7.5 % |
Titan | 0.25 % Show Material materials with Titan of 0.25 % |
Zink | 0.35 % Show Material materials with Zink of 0.35 % |