Thermisch
Property | Value |
---|---|
Schmelzpunkt | 546 - 621 °C Show Material materials with Schmelzpunkt of 546 - 621 °C |
Chemical properties
Property | Value |
---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Kupfer | 1.5 % Show Material materials with Kupfer of 1.5 % |
Magnesium | 0.6 % Show Material materials with Magnesium of 0.6 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Silizium | 5.5 % Show Material materials with Silizium of 5.5 % |
Titan | 0.25 % Show Material materials with Titan of 0.25 % |
Zink | 0.35 % Show Material materials with Zink of 0.35 % |