Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.64 g/cm³ Show Material materials with Dichte of 2.64 g/cm³ | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | |
20.0 °C | 2.64 g/cm³ Show Material materials with Dichte of 2.64 g/cm³ | H36 | EN 573-3 | Tube |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | A50 | |
2.0 % Show Material materials with Dehnung of 2.0 % | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | A100 | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | H36 | EN 573-3 | Tube | A50 | |
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | H36 | EN 573-3 | Tube | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 27.0 GPa Show Material materials with Schubmodule of 27.0 GPa | H36 | EN 573-3 | Tube | |
Zugfestigkeit | 320.0 MPa Show Material materials with Zugfestigkeit of 320.0 MPa | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
20.0 °C | 320.0 MPa Show Material materials with Zugfestigkeit of 320.0 MPa | H36 | EN 573-3 | Tube |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | -50 °C | 2.2499999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2499999999999998e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | |
-50.0 °C | 2.25e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.25e-05 1/K | H36 | EN 573-3 | Tube | ||
20 °C | 2.2499999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2499999999999998e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
20 °C | 2.41e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.41e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
20 °C | 2.51e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.51e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
20 °C | 2.61e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.61e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
100 °C | 2.41e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.41e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
100.0 °C | 2.41e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.41e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
200 °C | 2.51e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.51e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
200.0 °C | 2.51e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.51e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
300 °C | 2.61e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.61e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
300.0 °C | 2.61e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.61e-05 1/K | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Schmelzpunkt | 575.0 - 630.0 °C Show Material materials with Schmelzpunkt of 575.0 - 630.0 °C | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
Spezifische Wärmekapazität | 904.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 904.0 J/(kg·K) | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | ||
20.0 °C | 904.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 904.0 J/(kg·K) | H36 | EN 573-3 | Tube | ||
Wärmeleitfähigkeit | 20.0 °C | 110.0 - 140.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 110.0 - 140.0 W/(m·K) | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 15000000.0 - 19000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 15000000.0 - 19000000.0 S/m | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
spezifischer Widerstand | 5.26e-08 - 6.67e-08 Ω·m Show Material materials with spezifischer Widerstand of 5.26e-08 - 6.67e-08 Ω·m | H36 | EN 573-3, EN 754 | Rod, Tube, Wire |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | H36 | EN 573-3 | Tube |
0.50 % Show Material materials with Eisen of 0.50 % | H36 | EN 573-3, EN 754 | Rod, Tube, Wire | |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Magnesium | 4.5 - 5.6 % Show Material materials with Magnesium of 4.5 - 5.6 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Mangan | 0.1 - 0.6 % Show Material materials with Mangan of 0.1 - 0.6 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | H36 | EN 573-3, EN 754 | Tube, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): poor / poor, friction soldering: acceptable, soft brazing with flux: poor | |
Corrosion properties | Seawater: very good, weathering: very good | |
Workability | Bending / Spinning (cold): good / sufficient, Impact extrusion (cold): poor, Deep drawing / upsetting (Condition) good (O) / good (O) |