Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.6 - 2.7 g/cm³ Show Material materials with Dichte of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | F | EN 1706 | Casting | |
Elastizitätsmodul | 68.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Härte, Brinell | 70.0 [-] Show Material materials with Härte, Brinell of 70.0 [-] | F | EN 1706 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Zugfestigkeit | 250.0 MPa Show Material materials with Zugfestigkeit of 250.0 MPa | F | EN 1706 | Casting |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | F | EN 1706 | Casting | |
100 °C | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | F | EN 1706 | Casting | ||
Schmelzpunkt | 450.0 - 640.0 °C Show Material materials with Schmelzpunkt of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium | ||||
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium | ||||
Wärmeleitfähigkeit | 110.0 - 130.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 110.0 - 130.0 W/(m·K) | F | EN 1706 | Casting |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 14000000.0 - 16000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 14000000.0 - 16000000.0 S/m | F | EN 1706 | Casting |
spezifischer Widerstand | 6.25e-08 - 7.14e-08 Ω·m Show Material materials with spezifischer Widerstand of 6.25e-08 - 7.14e-08 Ω·m | F | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 89.83 % Show Material materials with Aluminium of 89.83 % | F | EN 1706 | |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % | F | EN 1706 | |
0.25 % Show Material materials with Eisen of 0.25 % | F | EN 1706 | Casting | |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % | F | EN 1706 | Casting |
Magnesium | 4.7 - 6.0 % Show Material materials with Magnesium of 4.7 - 6.0 % | F | EN 1706 | Casting |
Mangan | 0.4 - 0.8 % Show Material materials with Mangan of 0.4 - 0.8 % | F | EN 1706 | Casting |
Silizium | 1.8 - 2.6 % Show Material materials with Silizium of 1.8 - 2.6 % | F | EN 1706 | Casting |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | F | EN 1706 | Casting |
Zink | 0.07 % Show Material materials with Zink of 0.07 % | F | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: excellent | |
General machinability | as cast: excellent | |
Processing methods | pressure die casting, separately cast test sample |