Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.75 g/cm³ Show Material materials with Dichte of 2.75 g/cm³ | Typical for Cast 1xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Cast 1xx.x Series Aluminium | ||
Härte, Brinell | 75.0 [-] Show Material materials with Härte, Brinell of 75.0 [-] | T5 | GB 1173 | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 1xx.x Series Aluminium | ||
Zugfestigkeit | 165.0 MPa Show Material materials with Zugfestigkeit of 165.0 MPa | T5 | GB 1173 | |
175.0 MPa Show Material materials with Zugfestigkeit of 175.0 MPa | T5 | GB 1173 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.8e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8e-05 - 2.4e-05 1/K | Typical for Cast 1xx.x Series Aluminium |
Schmelzpunkt | 643.0 - 657.0 °C Show Material materials with Schmelzpunkt of 643.0 - 657.0 °C | Typical for Cast 1xx.x Series Aluminium |
Wärmeleitfähigkeit | 209.0 - 222.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 209.0 - 222.0 W/(m·K) | Typical for Cast 1xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Eisen | 0.60 % Show Material materials with Eisen of 0.60 % | T5 | GB 1173 |
Magnesium | 0.15 - 0.25 % Show Material materials with Magnesium of 0.15 - 0.25 % | T5 | GB 1173 |
Mangan | 0.9 - 1.2 % Show Material materials with Mangan of 0.9 - 1.2 % | T5 | GB 1173 |
Nickel | 0.2 - 0.3 % Show Material materials with Nickel of 0.2 - 0.3 % | T5 | GB 1173 |
Silizium | 1.6 - 2.0 % Show Material materials with Silizium of 1.6 - 2.0 % | T5 | GB 1173 |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | T5 | GB 1173 |
Zirkonium | 0.15 - 0.25 % Show Material materials with Zirkonium of 0.15 - 0.25 % | T5 | GB 1173 |