Chemical properties
Property | Value |
---|---|
Aluminium | 1.6 - 2.6 % Show Material materials with Aluminium of 1.6 - 2.6 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kupfer | 0.01 % Show Material materials with Kupfer of 0.01 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |