Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 9.5 % Show Material materials with Aluminium of 8.5 - 9.5 % |
Eisen | 4E-3 % Show Material materials with Eisen of 4E-3 % |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % |
Mangan | 0.17 % Show Material materials with Mangan of 0.17 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 0.45 - 0.9 % Show Material materials with Zink of 0.45 - 0.9 % |