Chemical properties
Property | Value |
---|---|
Eisen | 0.01 % Show Material materials with Eisen of 0.01 % |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % |
Lithium | 0.2 % Show Material materials with Lithium of 0.2 % |
Mangan | 0.15 % Show Material materials with Mangan of 0.15 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Seltene-Erden-Elemente | 1.5 - 4 % Show Material materials with Seltene-Erden-Elemente of 1.5 - 4 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Yttrium | 4.75 - 5.5 % Show Material materials with Yttrium of 4.75 - 5.5 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |
Zirkonium | 0.1 - 1 % Show Material materials with Zirkonium of 0.1 - 1 % |