Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % |
Eisen | 0.03 % Show Material materials with Eisen of 0.03 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 0.05 - 0.4 % Show Material materials with Mangan of 0.05 - 0.4 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.5 - 1.5 % Show Material materials with Zink of 0.5 - 1.5 % |