Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Material materials with Dichte of 1.74 g/cm³ | Typical for Pure Magnesium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 40 - 45 GPa Show Material materials with Elastizitätsmodul of 40 - 45 GPa | Typical for Pure Magnesium |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 - 2.6E-5 1/K | Typical for Pure Magnesium |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Pure Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1010 - 1050 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1010 - 1050 J/(kg·K) | Typical for Pure Magnesium |
Wärmeleitfähigkeit | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 153 - 167 W/(m·K) | Typical for Pure Magnesium |
Chemical properties
Property | Value |
---|---|
Aluminium | 4E-3 % Show Material materials with Aluminium of 4E-3 % |
Andere | each 0.005, For applications in nuclear energy technology: cadmium and boron should be limited to: Ca 0.0001 or 0.00005. B 0.00007 or 0.00003 |
Blei | 1E-3 % Show Material materials with Blei of 1E-3 % |
Bor | 3E-5 % Show Material materials with Bor of 3E-5 % |
Eisen | 2E-3 % Show Material materials with Eisen of 2E-3 % |
Kupfer | 5E-4 % Show Material materials with Kupfer of 5E-4 % |
Magnesium | 99.98 % Show Material materials with Magnesium of 99.98 % |
Mangan | 2E-3 % Show Material materials with Mangan of 2E-3 % |
Nickel | 5E-4 % Show Material materials with Nickel of 5E-4 % |
Silizium | 3E-3 % Show Material materials with Silizium of 3E-3 % |
Titan | 1E-3 % Show Material materials with Titan of 1E-3 % |