Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Material materials with Dichte of 1.74 g/cm³ | Typical for Magnesium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 45 GPa Show Material materials with Elastizitätsmodul of 45 GPa | Typical for Magnesium |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Wärmeleitfähigkeit | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 153 - 167 W/(m·K) | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Aluminium | 4.5 - 5.5 % Show Material materials with Aluminium of 4.5 - 5.5 % |
Andere | each 0.01. Rest Mg, This alloy is a patented alloying composition for elevated temperature applications., if the minimum Mn or maximum Fe content does not meet the specifications, then the Fe/Mg ratio must not exceed 0.021 |
Beryllium | 5E-4 - 1.5E-3 % Show Material materials with Beryllium of 5E-4 - 1.5E-3 % |
Eisen | 4E-3 % Show Material materials with Eisen of 4E-3 % |
Kupfer | 0.01 % Show Material materials with Kupfer of 0.01 % |
Mangan | 0.24 - 0.6 % Show Material materials with Mangan of 0.24 - 0.6 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silizium | 0.08 - 0.1 % Show Material materials with Silizium of 0.08 - 0.1 % |
Zink | 0.2 - 0.22 % Show Material materials with Zink of 0.2 - 0.22 % |