Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7 g/cm³ Show Material materials with Dichte of 7 g/cm³ | Typical for Cast/Wrought Aluminium Zinc Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 40 - 45 GPa Show Material materials with Elastizitätsmodul of 40 - 45 GPa | Typical for Cast/Wrought Aluminium Zinc Grade |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 - 2.6E-5 1/K | Typical for Cast/Wrought Aluminium Zinc Grade |
Schmelzpunkt | 365 - 645 °C Show Material materials with Schmelzpunkt of 365 - 645 °C | Typical for Cast/Wrought Aluminium Zinc Grade | |
Spezifische Wärmekapazität | 23.0 °C | 800 - 1100 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 800 - 1100 J/(kg·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Wärmeleitfähigkeit | 23.0 °C | 44 - 110 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 - 110 W/(m·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.3 - 9.7 % Show Material materials with Aluminium of 8.3 - 9.7 % |
Andere | each 0.02. Rest Mg, if the minimum Mn or maximum Fe content does not meet the specifications, then the Fe/Mg ratio must not exceed 0.032,each 0.01. Rest Mg, if the minimum Mn or maximum Fe content does not meet the specifications, then the Fe/Mg ratio must not exceed 0.032 |
Beryllium | 5E-4 - 1.5E-3 % Show Material materials with Beryllium of 5E-4 - 1.5E-3 % |
Eisen | 4E-3 - 5E-3 % Show Material materials with Eisen of 4E-3 - 5E-3 % |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % |
Mangan | 0.15 - 0.5 % Show Material materials with Mangan of 0.15 - 0.5 % |
Nickel | 1E-3 - 2E-3 % Show Material materials with Nickel of 1E-3 - 2E-3 % |
Silizium | 0.08 - 0.1 % Show Material materials with Silizium of 0.08 - 0.1 % |
Zink | 0.35 - 1 % Show Material materials with Zink of 0.35 - 1 % |