Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Material materials with Dichte of 1.74 g/cm³ | Typical for Magnesium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 45 GPa Show Material materials with Elastizitätsmodul of 45 GPa | Typical for Magnesium |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Wärmeleitfähigkeit | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 153 - 167 W/(m·K) | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Andere | total 0.30. Rest Mg, The rare earth metals should consist of didymium and not less than 70 % Neodymium and the rest from Praesodymium,total 0.0. Rest Mg, Rare earth metals should consist of didymium and not less than 70 % neodymium and the balance praseodymium |
Kupfer | 0.03 - 0.1 % Show Material materials with Kupfer of 0.03 - 0.1 % |
Mangan | 0.15 % Show Material materials with Mangan of 0.15 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Silber | 2 - 3 % Show Material materials with Silber of 2 - 3 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |
Zirkonium | 0.3 - 1 % Show Material materials with Zirkonium of 0.3 - 1 % |