Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 11.34 g/cm³ Show Material materials with Dichte of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 327 °C Show Material materials with Schmelzpunkt of 327 °C | Typical for Pure/Low Alloyed Lead | |
Spezifische Wärmekapazität | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Wärmeleitfähigkeit | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Andere | Other impurities: Total 0.1. Rest Pb,, The hardening of Pb-Sb alloys can be improved by arsenic, for semi-finished products 0.04 to 0.06 % As is recommended. |
Antimon | 0.3 - 0.7 % Show Material materials with Antimon of 0.3 - 0.7 % |
Arsen | 0.01 % Show Material materials with Arsen of 0.01 % |
Bismut | 0.05 % Show Material materials with Bismut of 0.05 % |
Kupfer | 5E-3 % Show Material materials with Kupfer of 5E-3 % |
Silber | 8E-3 % Show Material materials with Silber of 8E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 5E-3 % Show Material materials with Zinn of 5E-3 % |