Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9.8 g/cm³ Show Material materials with Dichte of 9.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 23.0 °C | 18 [-] Show Material materials with Härte, Brinell of 18 [-] |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Andere | Other impurities: Total 0.1. individually 0.03. Rest Pb., The age hardening of Pb-Sb alloys can be improved by arsenic, for casting alloys 0.08 to 0.15 % As are recommended. |
Antimon | 8 - 11 % Show Material materials with Antimon of 8 - 11 % |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Bismut | 0.05 % Show Material materials with Bismut of 0.05 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % |
Silber | 8E-3 % Show Material materials with Silber of 8E-3 % |
Zinn | 4 - 6 % Show Material materials with Zinn of 4 - 6 % |