Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 11 g/cm³ Show Material materials with Dichte of 11 g/cm³ |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 304 - 310 °C Show Material materials with Schmelzpunkt of 304 - 310 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Wärmeleitfähigkeit | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 - 57 W/(m·K) | Typical for Lead Tin |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | Rest Pb |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % |
Arsen | 0.03 % Show Material materials with Arsen of 0.03 % |
Bismut | 0.1 % Show Material materials with Bismut of 0.1 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % |
Gold | 0.05 % Show Material materials with Gold of 0.05 % |
Indium | 0.1 % Show Material materials with Indium of 0.1 % |
Kupfer | 0.08 % Show Material materials with Kupfer of 0.08 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Silber | 1.5 - 2 % Show Material materials with Silber of 1.5 - 2 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 1 - 3 % Show Material materials with Zinn of 1 - 3 % |