Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.28 g/cm³ Show Material materials with Dichte of 7.28 g/cm³ | Typical for Pure/Low Alloyed Tin |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 - 2.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 - 2.9E-5 1/K | Typical for Pure/Low Alloyed Tin |
Schmelzpunkt | 232 °C Show Material materials with Schmelzpunkt of 232 °C | Typical for Pure/Low Alloyed Tin | |
Spezifische Wärmekapazität | 23.0 °C | 205 - 238 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 205 - 238 J/(kg·K) | Typical for Pure/Low Alloyed Tin |
Wärmeleitfähigkeit | 23.0 °C | 52 - 74 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 52 - 74 W/(m·K) | Typical for Pure/Low Alloyed Tin |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | Total of all impurities: 0.100 |
Antimon | 0.04 % Show Material materials with Antimon of 0.04 % |
Arsen | 0.03 % Show Material materials with Arsen of 0.03 % |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 99.9 % Show Material materials with Zinn of 99.9 % |