Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.1 g/cm³ Show Material materials with Dichte of 7.1 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 50 GPa Show Material materials with Elastizitätsmodul of 50 GPa | Typical for Tin |
Poissonzahl | 23.0 °C | 0.36 [-] Show Material materials with Poissonzahl of 0.36 [-] | Typical for Tin |
Schubmodule | 23.0 °C | 18 GPa Show Material materials with Schubmodule of 18 GPa | Typical for Tin |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 - 2.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 - 2.9E-5 1/K | Typical for Tin |
Schmelzpunkt | 200 - 340 °C Show Material materials with Schmelzpunkt of 200 - 340 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 205 - 247 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 205 - 247 J/(kg·K) | Typical for Tin |
Wärmeleitfähigkeit | 23.0 °C | 52 - 74 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 52 - 74 W/(m·K) | Typical for Tin |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | Rest Sn |
Antimon | 0.1 % Show Material materials with Antimon of 0.1 % |
Arsen | 0.03 % Show Material materials with Arsen of 0.03 % |
Bismut | 0.1 % Show Material materials with Bismut of 0.1 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % |
Gold | 0.05 % Show Material materials with Gold of 0.05 % |
Indium | 0.1 % Show Material materials with Indium of 0.1 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Silber | 0.1 % Show Material materials with Silber of 0.1 % |
Zink | 39 - 41 % Show Material materials with Zink of 39 - 41 % |