Thermisch
Property | Value |
---|---|
Schmelzpunkt | 980 - 1060 °C Show Material materials with Schmelzpunkt of 980 - 1060 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Andere Beimengungen: zusammen 0,50, Rest Ni |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Bor | 2.75 - 3.5 % Show Material materials with Bor of 2.75 - 3.5 % |
Cadmium | 0.01 % Show Material materials with Cadmium of 0.01 % |
Chrom | 13 - 15 % Show Material materials with Chrom of 13 - 15 % |
Eisen | 4 - 5 % Show Material materials with Eisen of 4 - 5 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.6 - 0.9 % Show Material materials with Kohlenstoff of 0.6 - 0.9 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Selen | 5E-3 % Show Material materials with Selen of 5E-3 % |
Silizium | 4 - 5 % Show Material materials with Silizium of 4 - 5 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Zirkonium | 0.05 % Show Material materials with Zirkonium of 0.05 % |