Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.2 g/cm³ Show Material materials with Dichte of 9.2 g/cm³ | Typical for Nickel Molybdenum Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Nickel Molybdenum Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Molybdenum Alloy |
Schmelzpunkt | 1560 °C Show Material materials with Schmelzpunkt of 1560 °C | Typical for Nickel Molybdenum Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 439 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 439 J/(kg·K) | Typical for Nickel Molybdenum Alloy |
Wärmeleitfähigkeit | 23.0 °C | 9 - 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 9 - 15 W/(m·K) | Typical for Nickel Molybdenum Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 - 0.5 % Show Material materials with Aluminium of 0.1 - 0.5 % |
Andere | Nb + Ta 0.40 |
Chrom | 0.5 - 3 % Show Material materials with Chrom of 0.5 - 3 % |
Eisen | 1 - 6 % Show Material materials with Eisen of 1 - 6 % |
Kobalt | 3 % Show Material materials with Kobalt of 3 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 3 % Show Material materials with Mangan of 3 % |
Molybdän | 26 - 32 % Show Material materials with Molybdän of 26 - 32 % |
Nickel | 65 % Show Material materials with Nickel of 65 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Titan | 0.2 % Show Material materials with Titan of 0.2 % |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % |
Wolfram | 3 % Show Material materials with Wolfram of 3 % |