Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.7 g/cm³ Show Material materials with Dichte of 9.7 g/cm³ | Typical for Nickel Chromium Cobalt Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 240 GPa Show Material materials with Elastizitätsmodul of 240 GPa | Typical for Nickel Chromium Cobalt Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Cobalt Alloy |
Spezifische Wärmekapazität | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Cobalt Alloy |
Wärmeleitfähigkeit | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8 - 35 W/(m·K) | Typical for Nickel Chromium Cobalt Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 0.6 % Show Material materials with Aluminium of 0.3 - 0.6 % |
Andere | Rest Ni, Ti + Al 2.4 - 2.8 |
Bor | 5E-3 % Show Material materials with Bor of 5E-3 % |
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % |
Kobalt | 19 - 21 % Show Material materials with Kobalt of 19 - 21 % |
Kohlenstoff | 0.04 - 0.08 % Show Material materials with Kohlenstoff of 0.04 - 0.08 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.6 % Show Material materials with Mangan of 0.6 % |
Molybdän | 5.6 - 6.1 % Show Material materials with Molybdän of 5.6 - 6.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 1.9 - 2.4 % Show Material materials with Titan of 1.9 - 2.4 % |