Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.75 - 8.65 g/cm³ Show Material materials with Dichte of 7.75 - 8.65 g/cm³ | Typical for Nickel Chromium Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 150 - 245 GPa Show Material materials with Elastizitätsmodul of 150 - 245 GPa | Typical for Nickel Chromium Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Alloy |
Schmelzpunkt | 1400 °C Show Material materials with Schmelzpunkt of 1400 °C | Typical for Nickel Chromium Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Alloy |
Wärmeleitfähigkeit | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8 - 35 W/(m·K) | Typical for Nickel Chromium Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Andere | Rest Ni |
Bor | 0.01 % Show Material materials with Bor of 0.01 % |
Chrom | 20.5 - 23 % Show Material materials with Chrom of 20.5 - 23 % |
Eisen | 17 - 20 % Show Material materials with Eisen of 17 - 20 % |
Kobalt | 0.5 - 2.5 % Show Material materials with Kobalt of 0.5 - 2.5 % |
Kohlenstoff | 0.05 - 0.15 % Show Material materials with Kohlenstoff of 0.05 - 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 8 - 10 % Show Material materials with Molybdän of 8 - 10 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Wolfram | 0.2 - 1 % Show Material materials with Wolfram of 0.2 - 1 % |