Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.75 - 8.4 g/cm³ Show Material materials with Dichte of 7.75 - 8.4 g/cm³ | Typical for Nickel Chromium Iron Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 150 GPa Show Material materials with Elastizitätsmodul of 150 GPa | Typical for Nickel Chromium Iron Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Iron Alloy |
Schmelzpunkt | 1200 - 1480 °C Show Material materials with Schmelzpunkt of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Wärmeleitfähigkeit | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 2.4 - 3 % Show Material materials with Aluminium of 2.4 - 3 % |
Andere | Rest Ni |
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Eisen | 8 - 11 % Show Material materials with Eisen of 8 - 11 % |
Kohlenstoff | 0.2 - 0.4 % Show Material materials with Kohlenstoff of 0.2 - 0.4 % |
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.1 - 0.25 % Show Material materials with Titan of 0.1 - 0.25 % |
Yttrium | 0.05 - 0.15 % Show Material materials with Yttrium of 0.05 - 0.15 % |
Zirkonium | 0.01 - 0.1 % Show Material materials with Zirkonium of 0.01 - 0.1 % |