Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ | Typical for Pure/Low Nickel Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 220 GPa Show Material materials with Elastizitätsmodul of 190 - 220 GPa | Typical for Pure/Low Nickel Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Schmelzpunkt | 1400 - 1500 °C Show Material materials with Schmelzpunkt of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Wärmeleitfähigkeit | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Chemical properties
Property | Value |
---|---|
Andere | The nickel composition includes Co |
Antimon | 1E-4 % Show Material materials with Antimon of 1E-4 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 1E-4 % Show Material materials with Bismut of 1E-4 % |
Blei | 5E-4 % Show Material materials with Blei of 5E-4 % |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % |
Kobalt | 0.01 % Show Material materials with Kobalt of 0.01 % |
Kohlenstoff | 0.015 % Show Material materials with Kohlenstoff of 0.015 % |
Kupfer | 5E-3 % Show Material materials with Kupfer of 5E-3 % |
Mangan | 5E-4 % Show Material materials with Mangan of 5E-4 % |
Nickel | 99.96 % Show Material materials with Nickel of 99.96 % |
Phosphor | 1E-3 % Show Material materials with Phosphor of 1E-3 % |
Schwefel | 1.5E-3 % Show Material materials with Schwefel of 1.5E-3 % |
Selen | 2E-4 % Show Material materials with Selen of 2E-4 % |
Silber | 5E-4 % Show Material materials with Silber of 5E-4 % |
Tantal | 5E-4 % Show Material materials with Tantal of 5E-4 % |
Tellur | 1E-4 % Show Material materials with Tellur of 1E-4 % |
Thallium | 1E-4 % Show Material materials with Thallium of 1E-4 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 1E-4 % Show Material materials with Zinn of 1E-4 % |