Chemical properties
Property | Value |
---|---|
Andere | The nickel composition includes Co |
Antimon | 1E-3 % Show Material materials with Antimon of 1E-3 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 5E-4 % Show Material materials with Bismut of 5E-4 % |
Blei | 1E-3 % Show Material materials with Blei of 1E-3 % |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % |
Kobalt | 0.1 % Show Material materials with Kobalt of 0.1 % |
Kohlenstoff | 0.015 % Show Material materials with Kohlenstoff of 0.015 % |
Kupfer | 5E-3 % Show Material materials with Kupfer of 5E-3 % |
Nickel | 99.95 % Show Material materials with Nickel of 99.95 % |
Phosphor | 2E-3 % Show Material materials with Phosphor of 2E-3 % |
Schwefel | 2.5E-3 % Show Material materials with Schwefel of 2.5E-3 % |
Selen | 1E-3 % Show Material materials with Selen of 1E-3 % |
Silber | 5E-4 % Show Material materials with Silber of 5E-4 % |
Tellur | 5E-4 % Show Material materials with Tellur of 5E-4 % |
Thallium | 5E-4 % Show Material materials with Thallium of 5E-4 % |
Zink | 2E-3 % Show Material materials with Zink of 2E-3 % |
Zinn | 5E-4 % Show Material materials with Zinn of 5E-4 % |