Chemical properties
Property | Value |
---|---|
Aluminium | 1.5 % Show Material materials with Aluminium of 1.5 % |
Andere | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 92 % Show Material materials with Nickel of 92 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % |
Titan | 2 - 3.5 % Show Material materials with Titan of 2 - 3.5 % |